Welcome to the World of RSP!



RSP (Rapid Solidification Process) Tooling uses a system that is able to spray molten steel onto a ceramic negative. While the steel is spraying the ceramic negative must spin and change angle in order to create an even distribution. (See Diagram Below)

Once the spray is complete, a 30lb-40lb steel deposit is left on the ceramic which must be left alone for aproximatly 90 minutes to cool. After that period has passed, the below image is what is left over.

This newly formed pattern will now be sent to the machine shop where it can be cut to fit its designed application.